whilst in alberta, canada. i built some board bows from hickory that would not even register on my lowest setting on my meter, which is 6%.
the bows shot well, (with just reasonable set.) and i built at least 10 HBI- only one ever failed.
now that i live on the damp west coast. the same hickory in my shed is now measuring between 10 and 11%.
so the question is, should i dry it out some, or leave as is(i now have an oven buit to binghams specs).
what is the ideal m/c.
i will be using it for backings on bows.
thanks
wayne