Great start Bob.
Like the rest of the guys, the wrought/twist handle is a neat ideal.
Do have a suggestion to save your self some sanding and grinding after forging. Just in case you didn't know already. It's gonna sound crazy too, but it works.
I take it your probably forging with a ball peen and shop hammers like the rest of us start with. Those things are made for beating bearings out of hubs and breakin' stuff. They don't care if they leave a scuff.
Grind, sand and and polish the head and peen of you hammers as perfect as you can possibly get them. As good as you would a knife. Do the same with your anvil. Keep it as flat and smooth as you can. Any blemish in either will be stamped right into your work. GRRRR!
It sometimes takes some dummies...ah hum, not me though, a bunch of extra sanding to figure out what's going on. ;~)