In an effort to make better knives, I'm trying to get a more consistent process down with each blade. I was wondering when you guys that forge your blades do your normalizing/thermal cycling (3 reducing heat cycles, not annealing)?
I just forged some blades out and while they're relatively knife-shaped, I'm just not good enough to not have to do some more profiling w/ a grinder, etc. Do you normalize after that, or do you wait until you've already put in your bevels, etc.? Are there specific things to be gained if I did it just after they were profiled and before I file in the bevels? I think I've heard of some folks doing all the work til the blade's finished, then normalizing right before quenching?
Thanks for your thoughts.
Jeremy