I was just wondering if moisture content is important when building fiberglass bows? Should each lam be in that 8% to 12% range? Also can lams be cut from both sapwood and heartwood? Any information would be greatly appreciated and thanks in advance.


Chris
Experience is something that you do not get until right after you need it!!!

TGMM Family of the Bow

Offline strungstick

  • Trad Bowhunter
  • **
  • Posts: 97
Re: Questions about lams
« Reply #1 on: February 25, 2010, 12:12:00 AM »
I think that the moisture range from 6%-12% is pretty common.  I think in the glass laminate bow too high a moisture can cause some moisture to come out of the lam when heated and possibly cause a barrier from a good glue line.  
Sapwood and heartwood can be used in a glass bow.

Offline Jason Scott

  • Trad Bowhunter
  • **
  • Posts: 364
Re: Questions about lams
« Reply #2 on: February 25, 2010, 09:30:00 AM »
Yes it matters. I saw lams and store them inside my house a/c and heat for a week or so if it is too humid. I will final sand them to taper or parallel just before glue up.  The oposite is a problem to consider too. If they are good and dry when you glue up and you wait too long before you seal the bow and leave it in a place not environmentaly regulated until you get to work on it again you may find split glass where the wood swelled from absorbing moisture and the glass couldn't take it.