If the Urac failed, I can only assume a few things. Either the mix was wrong (not likely if he makes lots of bows) or the resin was on the verge of going bad (more likely), or perhaps the bow was left strung in an extremely hot area for an extended time, then stressed. I've had my bows and several others who use Urac have had theirs at MOJam during a hot year (over 100 deg.) with no problems.
BTW You can do a search for DAP Weldwood Resorcinol Glue and find it at a lot of places, but it looks like the Home Depot stores out your way sell it. Most marine supply stores have it too.