If I already have a bow that is backed with hickory or bamboo could I use direct heat and still put some reflex in it?
"He never promised that the cross would not be heavy and the hill wouldn't be hard to climb"
"I don't want to gain the whole world, and lose my soul"

10 Year Active Army Disabled Vet.

Offline eflanders

  • Trad Bowhunter
  • **
  • Posts: 699
Re: Heat bending question
« Reply #1 on: April 11, 2011, 11:00:00 PM »
I will not be held responsible for this response! Heat can damage the glue on a laminated bow but depending on the glue used, it can still be done.  There are a lot of variables to contend with such as: lam thicknesses, glue used, amount of bend needed and more.  If any of the lams exceed 1/8" I personally wouldn't try it!

Offline StoneAK

  • Trad Bowhunter
  • **
  • Posts: 432
Re: Heat bending question
« Reply #2 on: April 12, 2011, 12:04:00 AM »
I used smooth on glue on this bow. I do not want to damage the bow but I would like to add reflex thanks for the response
"He never promised that the cross would not be heavy and the hill wouldn't be hard to climb"
"I don't want to gain the whole world, and lose my soul"

10 Year Active Army Disabled Vet.

Online Pat B

  • TG HALL OF FAME
  • Trad Bowhunter
  • *****
  • Posts: 15027
Re: Heat bending question
« Reply #3 on: April 12, 2011, 09:44:00 AM »
You might get some reflex in it but you also risk deteriorating the glue. I think I'd leave that bow as is and make another the way you want it.
Make the most of all that comes and the least of all that goes!
TGMM Family of the Bow

Offline StoneAK

  • Trad Bowhunter
  • **
  • Posts: 432
Re: Heat bending question
« Reply #4 on: April 12, 2011, 10:05:00 AM »
Thanks Pat and eflanders I figured thats what I would do. I have a caul design that DVS Hunter sent to me and I am going to give it a try.
"He never promised that the cross would not be heavy and the hill wouldn't be hard to climb"
"I don't want to gain the whole world, and lose my soul"

10 Year Active Army Disabled Vet.

Online Pat B

  • TG HALL OF FAME
  • Trad Bowhunter
  • *****
  • Posts: 15027
Re: Heat bending question
« Reply #5 on: April 12, 2011, 10:50:00 AM »
You might check with the manufacturer of the Smooth On to see what the effects of the heat will do and at what temp it will be adversely affected. I did this with the folks that make TiteBond glues because I wanted to remove a faulty backing from a bow. The tech support guy told me that TB glues will release at 150deg(F) so I knew I could heat it to that temp and sucessfully remove the backing to replace it. Most of these companies have a 1-800 number to call and I have found them very helpful.
Make the most of all that comes and the least of all that goes!
TGMM Family of the Bow

Users currently browsing this topic:

0 Members and 1 Guest are viewing this topic.
 

Contact Us | Trad Gang.com © | User Agreement

Copyright 2003 thru 2024 ~ Trad Gang.com ©