Author Topic: Titebond on glass bow  (Read 552 times)

Offline alex b

  • Trad Bowhunter
  • **
  • Posts: 104
Titebond on glass bow
« on: April 16, 2011, 08:01:00 PM »
I know people use titebond III on BBI's and BBO's but have never seen it used on glass laminates. Is it okay to use?

thanks
alex

Offline John Lipinski

  • Trad Bowhunter
  • **
  • Posts: 219
Re: Titebond on glass bow
« Reply #1 on: April 16, 2011, 08:19:00 PM »
In short, no.


There's a reason why you never see it used on glass.
Titebond is a woodglue--it won't bond well enough to fiberglass to make a trustworthy bow. I doubt it'd stay together if you stressed it to full draw, let alone last a long time.

Smooth-on is the standard for glass.

Offline JamesV

  • Trad Bowhunter
  • **
  • Posts: 2027
Re: Titebond on glass bow
« Reply #2 on: April 16, 2011, 08:25:00 PM »
What John said. I tried it, titebond will NOT hold on glass.  

James...............
Proud supporter of Catch a Dream Foundation
-----------------------------------
When you are having a bad day always remember: Everyone suffers at their own level.

Offline alex b

  • Trad Bowhunter
  • **
  • Posts: 104
Re: Titebond on glass bow
« Reply #3 on: April 16, 2011, 08:36:00 PM »
Thanks for the replies. What are some other glues that you dont need a heat box for? If I remember correctly, smooth-on wont air dry.

alex

Offline fujimo

  • Trad Bowhunter
  • **
  • Posts: 3619
Re: Titebond on glass bow
« Reply #4 on: April 16, 2011, 08:55:00 PM »
it will air dry, and the spec sheets give the info. but check out the thread
"Is smooth-on this forgiving"- some info in there, by folks with a lot of experience
with regards to heat cure versus strength etc.

Offline John Lipinski

  • Trad Bowhunter
  • **
  • Posts: 219
Re: Titebond on glass bow
« Reply #5 on: April 17, 2011, 12:31:00 AM »
check some of the heat box buildalongs too, you don't need much. just some foam insulation with foil backing and some tape that can take the heat is all you need, plus some light bulbs. Search around a bit, there's a wealth of knowledge here. Personally, I'd trust it more with heat so long as it's cured for the proper amount of time. Either way will work, though.

Offline JamesV

  • Trad Bowhunter
  • **
  • Posts: 2027
Re: Titebond on glass bow
« Reply #6 on: April 18, 2011, 09:19:00 AM »
Alex...........

Lots of guys use smooth-on without heat and have great results. I do know the wasted glue is as hard as glass the next morning without heat and has to be chipped off any tools it is on.

James...........
Proud supporter of Catch a Dream Foundation
-----------------------------------
When you are having a bad day always remember: Everyone suffers at their own level.

Users currently browsing this topic:

0 Members and 1 Guest are viewing this topic.
 

Contact Us | Trad Gang.com © | User Agreement

Copyright 2003 thru 2024 ~ Trad Gang.com ©