Just got a yew stave done yesterday!
Before going ahead and doing this, there was a bend in the yew stave that needed to be removed, laying the stave on its side and holding on end down the other end was about 4-5" off the table, I heated it and got the bend out, then it all looked good to go, and so I went about as the video showed, before I started the stave hade some reflex in it, after I finished the reflex had turned into a bit of deflex, is this because of the moisture that was added to one side? Will it dry out?
Thanks,