really happy with the static tips so far- great glue lines
after chatting to mark this morning- gonna have to go real slow around these tips, and just figure out how much i can take off, it going to almost be like working on a self bow- creeping up on the final desired thickness, a bit at a time.
i am going to use marks trick with the thread and the string wax- to see exactly when the tips start to flex.
been thinking about removing material until it just starts to flex, then adding a thin phenolic underlay on the tips,
1. to bring back some stiffnness.
2. to allow me to sand in a longitudinal string groove, without violating the glass, and
3. hopefully adding some stability
i have phenolic and the left over 030 ul glass from the layup- which do you think would be better?
i could put it through the sander to thin it down some??
i really want to keep the weight down- but still retain stability
maybe next time i will use uls glass- its my first recurve- so didnt even think about it when i ordered the glass