hiya all,
i have just got off the phone with the manufacturer/supplier. he is rearing to go- he has sent me samples of 1.5" and 1.75" glass. i will laminate them up to some dark veneers- get some good professional quality pics( mate is a pro photogragher).
and then post them up here- and then we can work out how things are going to go forward from here.
any suggestions as to what i should laminate them to, just to get a good visual of whats there.
maybe i should just glue them up to some solid black glass or something. or maybe satin some uniform wood, a very dark brown, and then glue it up.
any other tests ?
maybe a weight?
possibly a rudimentary stiffness test. he said that, on a 45# recurve he uses .015 less stack, than if he uses gordons - because of the higher glass content in the layup, and subsequent stiffness.
we will just have to wait now for when the samples arrive :D tic,toc....