Hey guys, I did a couple of bows last summer and tested the peel resistance. It did seem to have a better bond than 1-1. I also noticed that for me it seems that uls bonds better than ul. Not sure why but it does seem to bond slightly better.
Anyways, I have adopted this as standard procedure simply because of the increased peel and heat resistance. I’ve done approximately 20 Bows this way and have no complaints, although I didn’t have any complaints before either.
A little more glue is worth a little more piece of mind I guess. Lol