Author Topic: Heat treating and unibond?  (Read 1394 times)

Offline John Malone

  • Trad Bowhunter
  • **
  • Posts: 699
Heat treating and unibond?
« on: April 16, 2018, 05:40:13 PM »
He guys, just wondering if you can heat treat a belly after a bamboo backing was added using unibond?
Life is to short to pass up anything that could potentially be bow wood!

Online Roy from Pa

  • Administrator
  • Trad Bowhunter
  • ****
  • Posts: 20686
Re: Heat treating and unibond?
« Reply #1 on: April 16, 2018, 06:08:34 PM »
Yup, just don't over heat.

Offline Wolftrail

  • Trad Bowhunter
  • **
  • Posts: 1152
Re: Heat treating and unibond?
« Reply #2 on: April 16, 2018, 06:33:24 PM »
Yup, just don't over heat.
Sure enough I have heated laminated  limbs for twist correction and the glue held.

Offline John Malone

  • Trad Bowhunter
  • **
  • Posts: 699
Re: Heat treating and unibond?
« Reply #3 on: April 16, 2018, 08:55:48 PM »
Thanks guys. Just need to touch it up so to speak.
Life is to short to pass up anything that could potentially be bow wood!

Offline Eric Krewson

  • Trad Bowhunter
  • **
  • Posts: 3126
Re: Heat treating and unibond?
« Reply #4 on: April 17, 2018, 09:14:05 AM »
I often bend handles to align the limbs, I never had a handle glued on with the old Urac turn loose but did have one glued on with unibond turn loose.