Thats exactly right Stic, you are only going to get so much saturation with a wet layup, when not wetting out each layer individually.
Plus the fiber/resin volume fraction is going to be at the lowest end of the scale in an open layup. There is going to be a lot of surface finishing going on here, considering all the visible surface voids.